Figure 6 Calculated (1) and experimental, determined by the hydrostatic method
(2) density of organoplastics
Source: developed by the author
Figure 7 Compression curves of organoplastics based on PFR and containing:
60 mass.% of Rusar fiber (1); 60 (2) and 70 (3) mass.% of Tanlon fiber
Source: developed by the author
Figure 8 The character of the destruction of the samples after compression;
the samples contain: 60 mass.% of fiber Rusar (a), 60 (b) and 70 (c) mass.%
of Tanlon fiber
Source: developed by the author